On the specification sheet of soft magnetic absorbing materials, the tangent of magnetic loss angle and the peak value of μ "are usually placed in the most prominent position. A sheet-like FeSiAl composite material, with a peak of μ "around 10 GHz and a magnetic loss tangent exceeding 0.5, appears to be sufficient to support the conclusion of" efficient absorption ".
But when the engineer applied this material to the metal backplate to measure the reflection loss, the results did not match the peak value specified in the specifications: the peak value was several dB lower, or the peak frequency was shifted, or the absorption bandwidth was significantly narrowed. Retesting the magnetic loss, there are no issues with the data. The problem lies in another parameter: dielectric constant.
Reflection loss is determined by two conditions, and magnetic loss is just one of them
The reflection loss of absorbing materials depends on the product of two conditions: whether electromagnetic waves can enter the interior of the material, and whether the electromagnetic waves entering the interior of the material can be effectively attenuated.
The first condition: Impedance matching determines whether "entry is possible"
The wave impedance of free space is about 377 Ω. The closer the input impedance of the material is to this value, the lower the proportion of incident electromagnetic waves reflected and the more energy enters the interior of the material. The input impedance of a material is determined by both the complex dielectric constant and the complex magnetic permeability, and is roughly proportional to √ (μ/ε). If ε 'is much higher than μ', the input impedance is low, mismatched with free space, and the reflection is enhanced.
The second condition: The loss mechanism determines whether it can attenuate
Electromagnetic waves entering the interior of materials are converted into thermal energy through magnetic and dielectric losses. The absolute values of μ "and ε" determine the amount of attenuation per unit length.
Both conditions are indispensable. If only the second condition (high μ ") is met and the first condition (impedance mismatch) is not met, the electromagnetic wave will be reflected back on the surface, and μ" will not have a chance to play a role. This is the physical reason why the magnetic loss meets the standard and the reflection loss is very poor.
Why is the dielectric constant of soft magnetic powder relatively high
The commonly used powders for soft magnetic absorbing materials, such as sheet-like FeSiAl, carbonyl iron powder, and metal soft magnetic alloy powder, are themselves conductors or semiconductors with naturally high dielectric constants. After flaking, the specific surface area of the powder increases, the contribution of surface oxide layer and interface polarization increases, and ε 'further increases. In the composite matrix, if the powder filling amount is high (in order to obtain sufficient μ 'and μ' '), the interface polarization and dipole polarization between particles will further increase the effective ε'.
The influence of high ε 'on incident energy
The result is that a piece of soft magnetic absorbing material with excellent magnetic loss data may have an ε 'in the range of 20-50 or even higher. In the X-band (8-12 GHz), the input impedance of the material corresponding to ε'30 is much lower than 377 Ω, and the reflection coefficient may exceed 0.5. More than half of the incident energy is reflected on the surface, and less than half enters the material's interior to participate in magnetic loss.
Why does the peak reflection loss on the specification sheet shrink in the entire machine
The reflection loss data on the specification sheet is usually measured under specific testing conditions: the material is attached to a metal backplate and measured using waveguide or bow method. This testing condition itself already includes the impact of impedance mismatch - the reason why the peak can still be seen is often because the thickness of the test sample happens to fall near a certain phase cancellation point, or the material's ε 'is partially compensated by some mechanism in the testing frequency band.
However, in the application of the whole machine, there are differences between the mounting conditions and testing conditions: the material and area of the metal backplate are different, the distance between the material and the antenna is different, and there are other media or metal structures around it. These differences will alter the equivalent environment of the input impedance of the material, and the impedance matching that was initially barely established under testing conditions may further deteriorate under overall machine conditions. The "shrinkage" of the peak reflection loss is essentially the result of switching from "specific matching conditions in the laboratory" to "actual mismatch conditions of the entire machine".
'Magnetic loss illusion': why high μ 'does not equal strong absorption
How many electromagnetic waves have entered the material
The term 'μ' describes the magnetic loss capacity per unit volume within a material, but it does not describe 'how many electromagnetic waves enter this volume'. A material with a high μ "but also extremely high ε 'has very few electromagnetic waves entering its interior, and the actual total energy absorbed may be lower than that of a material with a medium μ" but controlled ε'. This is the source of the 'magnetic loss illusion': when selecting, only the peak value of μ 'is considered, ignoring the constraint of ε' on energy entry efficiency. In the systems of flake powder and metal soft magnetic powder, this illusion is particularly common - flaking increases both μ "and ε ', and the two effects cancel each other out. The actual improvement in reflection loss is much lower than the amplitude implied by the increase in μ".
Three pathways for regulating dielectric constant
To improve impedance matching while maintaining magnetic losses, it is necessary to regulate ε 'in engineering. Three common paths:
Firstly, the surface is coated with a low dielectric layer
Coat the surface of the powder with a low dielectric constant and low loss insulation layer (such as SiO ₂, Al ₂ O3, polymer) to reduce interfacial polarization between particles, while cutting off the conductive path between particles and reducing effective ε '. The thickness of the coating layer needs to match the particle size and filling amount of the powder - too thin, insufficient insulation; Excessive thickness dilutes the volume fraction of magnetic fillers.
Secondly, porosity
Introducing pores into the material and utilizing the low dielectric constant of air (ε '≈ 1) to lower the effective ε' of the composite material. The porous structure also increases the reflection path of electromagnetic waves inside the material, prolongs the propagation path, and makes additional contributions to absorption. However, porosity will reduce the mechanical strength and magnetic permeability of the material, and the porosity needs to be balanced with the target frequency band and thickness constraints.
Thirdly, gradient packing distribution
Construct a gradient of filler concentration in the thickness direction, so that the surface of the material has a lower ε '(close to free space) and the internal ε' is higher. The impedance changes encountered by electromagnetic waves entering from the surface are smoother and the reflection is reduced; After entering the interior, the high packing concentration area provides sufficient loss. The implementation methods of gradient include multi-layer stacking and centrifugal/magnetic field assisted molding.
Selection and judgment of soft magnetic absorbing materials based on impedance matching
Firstly, suppliers are required to provide data on the target frequency band including μ ', μ', ε′, and ε″, rather than just providing magnetic loss parameters
μ 'alone cannot predict reflection loss, while ε' determines whether electromagnetic waves can enter the material. If the supplier can only provide magnetic loss tangent or peak value, the risk of impedance matching cannot be evaluated.
Secondly, evaluate the material using the product of the attenuation constant multiplied by the matching efficiency, rather than just looking at the peak loss
The attenuation constant describes the attenuation rate of electromagnetic waves entering a material, while the matching efficiency describes how much energy enters the material. The product of the two corresponds to the actual reflection loss. In engineering, suppliers can be required to provide the reflectivity curve of the target frequency band and confirm whether the testing conditions (metal backplate material, sample thickness, testing method) are comparable to the overall application conditions of the machine.
Thirdly, in the scheme of flake powder and metal soft magnetic powder, the control of dielectric constant is considered as an independent selection dimension
Flakiness and high filling content will increase both μ 'and ε'. If the supplier does not provide instructions for dielectric constant control (coating, porosity, gradient), the risk of impedance mismatch needs to be independently verified. Suppliers can be requested to provide comparative data of ε 'between the' uncontrolled version 'and the' regulated version '.
Fourth, retest the reflection loss under the condition of complete machine mounting, rather than extrapolating from specification data
Impedance matching is sensitive to the mounting environment, and the peak values on the specification sheet are obtained under specific testing conditions. During the sample stage, the reflection loss or reading distance/shielding effectiveness should be retested under the actual metal substrate, actual spacing, and actual surrounding structural conditions to confirm the actual performance of the material in the overall environment.
Advanced Institute (Shenzhen) Technology Co., LtdThe product line of soft magnetic absorbing materials covers sheet-like FeSiAl and carbonyl iron powder composite systems, providing complete data on target frequency bands such as μ ', μ', ε′, and ε″, as well as comparative data on reflection loss for three dielectric constant control schemes: surface coating, porosity, and gradient.
The product helps engineers extend the selection criteria from "peak magnetic loss" to "product of magnetic loss and impedance matching". For more technical information, please visithttp://www.avanzado.cn/.