Current:Home >Company news >Frontier News >Why does the contact pressure loosen first during the cooling stage when there is no adhesive buffer layer for the "thermal cycle breathing" of adhesive free copper foil tape
先进院(深圳)科技有限公司

Hotline:0755-22277778 Tel:0755-22277778 
Mobile:13826586185(Mr.Duan)
Fax:0755-22277776
E-mail:duanlian@xianjinyuan.cn

Frontier News

Why does the contact pressure loosen first during the cooling stage when there is no adhesive buffer layer for the "thermal cycle breathing" of adhesive free copper foil tape

Time:2026-11-16Number:13

The grounding reliability of adhesive free copper foil tape is usually confirmed during the sample stage by measuring the contact resistance after crimping. The crimping fixture applies a certain pressure, the copper foil comes into contact with the substrate, and the contact resistance meets the standard. The plan is approved.

This verification is completed under constant temperature conditions, with the implicit assumption that 'the contact pressure after crimping will remain constant'. But for scenarios that experience temperature cycling - in vehicles, outdoors, near power modules - the contact pressure is not constant. The adhesive free structure has no elastic recovery force of the adhesive layer to "compensate" for the displacement caused by thermal expansion, and the contact pressure between the copper foil and the substrate fluctuates with increasing and decreasing temperature. This fluctuation has a clear direction: the contact pressure during the cooling stage is more prone to relaxation than during the heating stage.

Thermal expansion mismatch: Copper foil swells and shrinks more than most metal substrates

The thermal expansion coefficient of copper is about 16-17 ppm/℃. Among common substrates, aluminum is about 23 ppm/℃, stainless steel is about 17 ppm/℃, and galvanized steel sheet is about 12-13 ppm/℃. The CTE of copper foil is similar to that of aluminum substrate, but differs from that of stainless steel and galvanized steel plate. However, more importantly, in the crimping structure, copper foil is usually very thin (0.018-0.05 mm) and the substrate is thicker. The thermal capacity and stiffness of thin copper foil are much lower than those of thick substrates. When the temperature changes, the expansion/contraction of copper foil is more easily "constrained" by the substrate, but the constraint process will generate stress at the interface.

Temperature stage Deformation trend of copper foil relative to substrate Interface stress Change in contact resistance
warm up Expand outward and be constrained by the substrate Increased compressive stress Possible temporary decrease (favorable)
cool down Shrink inward and generate relative displacement with the substrate Release of compressive stress, even turning to tensile stress Rising (contact point 'loosening')

When the temperature rises, if the expansion trend of copper foil is greater than that of the substrate, the copper foil at the interface "wants" to expand outward, but is constrained by the substrate, generating compressive stress and increasing contact pressure. When the temperature decreases, if the shrinkage trend of the copper foil is greater than that of the substrate, the copper foil at the interface "wants" to shrink inward, generating tensile stress between it and the substrate, and reducing the contact pressure. The premise of this analysis is that there is a difference in CTE between copper foil and substrate, and the deformation of copper foil is constrained by the substrate. In crimping structures, this premise usually holds true.

Cooling stage: release of compressive stress, loosening of contact points

During the heating stage, the interface compressive stress increases, and the micro protrusions of the copper foil are further pressed into the micro depressions of the substrate. The contact point density increases, and the contact resistance may temporarily decrease. This stage is advantageous for contact resistance.

Two layer effect during the cooling phase

During the cooling phase, the situation reverses. The compressive stress is released as the temperature decreases, and the micro protrusions of the copper foil "bounce back" from the depressions of the substrate, resulting in a decrease in contact point density and an increase in contact resistance. If the cooling amplitude is large enough, the interface may even transition from "compressive stress" to "tensile stress" - there is a slight separation trend between the copper foil and the substrate, the contact pressure approaches zero, and the contact resistance sharply increases.

The adhesive layer of the copper foil tape with adhesive plays a buffering role here: although the adhesive layer hardens during cooling, it still retains a certain degree of elasticity, which can compensate for some of the thermal shrinkage differences through its own deformation and maintain contact pressure. The adhesive free copper foil does not have this buffering layer, and the contact pressure relaxation during the cooling stage is more direct and significant.

The cumulative effect of "breathing": irreversible drift of contact resistance

In a single temperature cycle, the fluctuation of contact resistance may be reversible - it decreases during heating, increases during cooling, and returns to near initial value after returning to room temperature. But after multiple cycles, the cumulative effect begins to manifest.

Each time the compressive stress is released during the cooling stage, the micro protrusions of the copper foil undergo slight plastic deformation or wear. After dozens to hundreds of cycles, the shape of the micro protrusions is partially "smoothed", and even at room temperature, the same nominal pressure is still applied to the crimping fixture, resulting in a lower actual contact point density than the initial state. The 'room temperature value' of the contact resistance itself begins to drift upwards, rather than just fluctuating in cycles. This cumulative effect also exists in adhesive tape, but the elastic recovery force of the adhesive layer can partially offset the contact pressure loss caused by plastic deformation. The adhesive free structure does not have this compensation mechanism, and the accumulated drift is more pronounced.

Why can't the 'initial crimping pressure' predict the performance after cycling

The initial pressure is only the starting point, the remaining pressure is the key

The contact resistance measured during sample verification was obtained under initial crimping pressure and in a constant temperature environment. It describes the contact state at the moment after crimping. The contact resistance after temperature cycling depends on how much pressure is left after experiencing thermal cycling. This' residual pressure 'is determined by the initial crimping pressure, CTE difference, cycle amplitude, cycle number, and interface microstructure. The combination with the same initial crimping pressure, large CTE difference, scenarios with large cyclic amplitude, and interfaces with obvious micro convex plastic deformation changes have lower residual pressure and greater contact resistance drift. Therefore, for the selection verification of adhesive free copper foil tape, it is necessary to confirm the "contact pressure retention rate after thermal cycling" as an independent indicator, rather than extrapolating from the initial contact resistance.

Selection and assembly judgment based on "contact pressure retention rate after thermal cycling"

Firstly, suppliers are required to provide contact resistance data after thermal cycling, rather than just providing contact resistance data after initial crimping

The testing conditions should cover the low and high temperature endpoints of actual service, with a minimum of ten cycles. After testing, the contact resistance should be retested at room temperature and compared with the room temperature value before cycling. If the ambient temperature contact resistance after cycling rises beyond an acceptable range, it indicates that cumulative drift has occurred.

Secondly, introduce a "pressure compensation" mechanism in structural design to compensate for the lack of adhesive buffering in non adhesive structures

Elastic components such as waveform washers and spring plates can be added to the crimping structure to maintain the crimping pressure even when the copper foil undergoes thermal shrinkage. The stiffness of the elastic element needs to match the thickness and CTE difference of the copper foil - if the stiffness is too high, the compensation ability is insufficient; The stiffness is too low, and the initial crimping pressure is insufficient.

Thirdly, select copper foil surface treatment according to the CTE of the substrate to reduce interfacial friction and plastic deformation

The greater the difference in CTE between copper foil and substrate, the greater the relative displacement during the cooling stage, and the more significant the plastic deformation changes in interface friction and microscopic protrusions. The surface of tinned copper foil is more prone to plastic flow during crimping, which can fill more micro depressions, but at the same time, it is also easier to "smooth out" during cycling. For combinations with significant differences in CTE, it is necessary to confirm whether the coating thickness and hardness are suitable for the target number of cycles.

Fourthly, use "room temperature contact resistance after cycling" as the acceptance indicator during the sample stage, rather than "high-temperature contact resistance during cycling"

The relaxation of contact pressure during the cooling phase usually only fully manifests its consequences after returning to room temperature. After the temperature cycling test is completed, the lap resistance and shielding effectiveness should be retested at room temperature and compared with the room temperature data before cycling. If the performance at room temperature decreases beyond an acceptable range after cycling, it indicates that the contact pressure relaxation during the cooling stage has caused irreversible interface damage.

Advanced Institute (Shenzhen) Technology Co., LtdThe adhesive free copper foil tape product line covers bare copper and tin plated substrates, with a thickness range of 0.018-0.05 mm. It can provide contact resistance change data and contact pressure retention evaluation after temperature cycling from -40 ℃ to 125 ℃. It supports matching suggestions for copper foil surface treatment and crimping structure based on substrate CTE and cycling conditions.

For more technical information, please visithttp://www.avanzado.cn/.

Contact Us

Company: Xianjin Yuan (Shenzhen) Technology Co., Ltd.
Address: 8/F, Zhongxing Building, Shajing Xinsha Road, Bao'an District, Shenzhen, Guangdong, China
Tel: 0755-22277778  |  13826586185
Email: duanlian@xianjinyuan.cn
Website: http://www.avanzado.cn/
Related news
Hotline
0755-22277778
13826586185(Mr.Duan)
Wechat QRcode Wechat QRcode