Frontier News

The "cost of removing the adhesive layer" of adhesive free copper foil tape: why does the reliability of grounding rely more on interface management instead of adhesive

Time:2026-11-16Number:14

The appearance of adhesive free copper foil tape in BOM usually corresponds to a clear constraint: the adhesive layer cannot withstand it. The high temperature near reflow soldering, long-term service environments above 120 ℃, or clean environments that do not allow any organic matter to escape, will push the selection from "with glue" to "without glue".

This choice is correct in terms of temperature resistance. The temperature resistance bottleneck of copper foil tape with adhesive always lies in the adhesive layer: the long-term temperature resistance of ordinary acrylic pressure-sensitive adhesive is about 80-105 ℃, while modified acrylic can reach around 150 ℃. However, once the adhesive layer softens and crawls, the contact pressure relaxes, and the grounding impedance drifts accordingly. The adhesive free copper foil tape removes the variable of adhesive layer, and the temperature resistance of copper foil becomes the upper limit of the system. The temperature resistance range of the adhesive free form can cover the order of -50 ℃ to 1000 ℃. But 'removing the adhesive layer' does not mean 'removing the work that the adhesive layer originally undertook'.

The adhesive layer does two things in the adhesive tape, not just "sticking"

The adhesive layer of copper foil tape with adhesive is often simplified as "bonding". But in the grounding path, the adhesive layer actually plays two more critical engineering roles.

The first role is to provide and maintain contact pressure

The pressure-sensitive adhesive is pressed together during installation, and the elastic recovery force of the adhesive continues to press the copper foil against the surface to be attached. This pressure causes the microscopic protrusions on the copper foil surface to interlock with the microscopic depressions on the substrate surface, forming actual metal metal contact points. When the adhesive layer ages or creep, the pressure relaxes and the contact resistance increases - this is one of the main pathways for the long-term reliability degradation of adhesive tape.

The second role is to fill micro gaps

Even "flat" metal surfaces have roughness on the micrometer scale. The adhesive layer fills these depressions during compression, eliminating the air gap between the copper foil and the substrate. The electrical resistivity of air is actually infinite, and any unfilled gap contributes to the contact resistance.

The adhesive free copper foil tape removes the adhesive layer, and these two functions must be undertaken by other means. If they are not replaced, the copper foil is only "placed" on the metal surface, not "connected" to the metal surface.

Contact pressure: the first dominant variable for non adhesive grounding

The conductive path of adhesive free copper foil tape relies entirely on the direct physical contact between the copper foil and the substrate. The relationship between contact area and contact resistance is not "the larger the nominal area, the better", but "the more microscopic points where metal metal contact actually occurs, the better". The number of microscopic points is determined by the contact pressure.

The difference between insufficient pressure and sufficient pressure

When there is insufficient pressure:There are only a few highest micro protrusions in contact between copper foil and substrate, and the effective conductive cross-sectional area is much smaller than the geometric area, resulting in high and unstable contact resistance.

When the pressure is sufficient:More micro protrusions undergo plastic or elastic deformation, resulting in an increase in contact point density, a decrease in contact resistance, and a tendency towards stability.

Adhesive tape automatically provides this pressure through the elastic recovery force of the adhesive layer, while non adhesive tape does not have this automatic mechanism. The pressure must come from external sources: mechanical fixtures, compression structures, fasteners, or the fixing effect of welding/conductive adhesive. If the assembly design only places or covers the non adhesive copper foil on the metal surface without independent clamping means, the contact pressure depends entirely on gravity, assembly tolerances, and accidental interference, and the dispersion and long-term drift of the grounding impedance are uncontrollable.

Surface state: The oxide layer is a more critical variable than roughness

The contact pressure solves the problem of whether the microscopic protrusions can touch, while the surface state solves the problem of whether they can conduct electricity after touching.

The influence of oxide layer on contact resistance

Copper naturally forms an oxide layer in the air, and the electrical resistivity of cuprous oxide and cuprous oxide is much higher than that of metallic copper. Even if the contact pressure is sufficient to allow the protrusions of the copper foil to "touch" the substrate, if there is a layer of nanometer to micrometer scale oxide film between the two, the metal metal contact is not truly established. The adhesive free copper foil tape does not have conductive particles in the adhesive layer to "pierce" this oxide film. The cleanliness and degree of oxidation of the contact interface directly determine whether the grounding is established.

If the adhesive layer of the tape contains conductive particles, the particles can locally puncture the oxide layer under pressure; Non adhesive tape has no such mechanism at all. This means that adhesive free scenarios have higher requirements for surface pretreatment: mechanical polishing, chemical cleaning, or plasma treatment before mounting are not "optional process optimizations", but necessary steps to ensure proper grounding.

The surface condition of copper foil itself is equally important. Untreated bare copper foil surface oxidation during storage can reduce solderability and contact conductivity. Tin plated copper foil, under contact pressure, has a thinner and more fragile tin oxide film than copper oxide film, making it more susceptible to damage during lamination or welding processes. It is a more robust surface treatment option in adhesive free scenarios.

Overlapping and fixing: The "conductive path" of non adhesive tape must be explicitly defined in the assembly design

When the adhesive copper foil tape is overlapped, the conductivity of the adhesive layer (double conductivity) or the direct contact of the copper foil surface (single conductivity) provides a path for current to cross the joint. Adhesive free copper foil tape has no adhesive layer involved in conductivity, and the current crossing at the overlap completely depends on the direct contact between copper foils - and the direct contact between two layers of copper foils also requires pressure and surface cleaning.

Two electrical connection methods at the lap joint

Welding:Use solder metallurgy to connect the overlapping parts and eliminate the uncertainty of contact resistance.

Mechanical crimping:Apply and maintain sufficient pressure in the overlapping area using fixtures or fasteners.

If the overlap is only "stacking", the contact pressure between the two layers of copper foil only comes from the weight of the upper copper foil and the support of the lower substrate, and the contact point density is extremely low, the overlap resistance may be much higher than the resistance of the copper foil body. At high frequencies, the contact capacitance and contact inductance at the junction will also introduce additional impedance discontinuities. Without welding or mechanical crimping, the overlap of adhesive free copper foil is incomplete in electrical terms.

Selection and assembly judgment of adhesive free copper foil tape from the perspective of "mechanical interface"

Firstly, confirm whether there are independent sources of pressure in the assembly design before selecting the adhesive tape

The grounding reliability of adhesive free copper foil tape does not depend on the parameters of the tape itself, but on whether the assembly structure can provide and maintain sufficient contact pressure in the target contact area. If there are no fixtures, clamps, or welding designs in the structure, adhesive tape should not be selected as the only material for the grounding path.

Secondly, incorporate surface pretreatment into the process specifications, rather than relying on the intuition of "just stick it on"

In non adhesive scenarios, the oxide layer and contamination are the direct sources of contact resistance. Before installation, the copper foil and substrate surfaces should be cleaned (if necessary, mechanically polished or plasma treated), and the allowable interval between cleaning and installation should be clearly stated in the process document to avoid re oxidation of the cleaned surface.

Thirdly, choose copper foil surface treatment based on the service temperature, not just the purity of the copper foil

The upper limit of temperature resistance of adhesive free copper foil is determined by the copper foil itself, but the surface oxidation rate under long-term high temperature will affect the stability of contact resistance. The oxidation behavior of tinned copper foil at high temperatures is better than that of bare copper. For non adhesive scenarios above 100 ℃ for a long time, tinned or oxygen free copper is a more robust starting point.

Fourthly, the electrical connection method must be clearly defined at the lap joint and cannot rely on "stacking contact"

Require the design documents to specify the connection methods (welding, crimping, fasteners) for the overlap area, and measure the overlap resistance during the sample stage, rather than just measuring the contact resistance between the single-layer copper foil and the substrate. The overlap resistance is usually higher than the single-layer contact resistance and is a more easily underestimated link in the grounding path.

Advanced Institute (Shenzhen) Technology Co., LtdThe adhesive free copper foil tape product line covers bare copper and tin plated substrates, with a thickness range of 0.018-0.05 mm. It can provide copper foil surface resistivity (≤ 0.05 Ω/sq level) and contact resistance data under different crimping conditions. It supports providing assembly interface evaluation recommendations based on target contact pressure, surface state, and overlap method.

For more technical information, please visithttp://www.avanzado.cn/.

Contact Us

Company: Xianjin Yuan (Shenzhen) Technology Co., Ltd.
Address: 8/F, Zhongxing Building, Shajing Xinsha Road, Bao'an District, Shenzhen, Guangdong, China
Tel: 0755-22277778  |  13826586185
Email: duanlian@xianjinyuan.cn
Website: http://www.avanzado.cn/
Related news
Hotline
0755-22277778
13826586185(Mr.Duan)
Wechat QRcode Wechat QRcode