Current:Home >Company news >Frontier News >Conductive adhesive copper foil tape: engineering selection from lap resistance to shielding effectiveness
先进院(深圳)科技有限公司

Hotline:0755-22277778 Tel:0755-22277778 
Mobile:13826586185(Mr.Duan)
Fax:0755-22277776
E-mail:duanlian@xianjinyuan.cn

Frontier News

Conductive adhesive copper foil tape: engineering selection from lap resistance to shielding effectiveness

Time:2026-11-18Number:22

Technical Note  /  Shielding Materials

There is a 0.3mm gap left at the edge of the shielding cover, and the overall radiation of the machine exceeds the limit around 800MHz. The engineer cut a circle of copper foil tape and stuck it along the seam, but the problem did not disappear. The reason is often not in the tape itself: the adhesive layer of ordinary copper foil tape is insulating, and it sticks the copper foil to the shielding cover, but does not remove the copper foilto pick upTo the shielding cover - there is a non-conductive adhesive layer between two metals, and the overlap resistance may be as high as megaohms, but the gap still exists electrically. After replacing with conductive adhesive copper foil tape and compacting the overlapping surface, the remaining amount at the same frequency point will return.

The key to this material has never been 'how thick the copper is', but ratherCopper foil - adhesive layer - stickerDo these three sections form a continuous low resistance pathway. Understanding this pathway means understanding the entire selection logic.

01Structure: Copper foil, conductive adhesive, release profile

A typical structure consists of only three layers: copper foil substrate, conductive adhesive layer, release film or release paper, supplied in the form of rolls or die cut parts. Copper foil is responsible for shielding and current carrying, adhesive layer is responsible for fixing and conducting, and only ensures that the profiles are not contaminated during transportation and die-cutting. It may seem simple, but the choice of each layer will change the final result.

Copper foilDivided into two types: rolled copper (RA) and electrolytic copper (ED). Rolled copper grains elongate along the rolling direction, with significantly better ductility and bending resistance. Repeated bending is less likely to crack, making it suitable for wrapping cables, attaching curved surfaces, and dynamic bending areas; Electrolytic copper has low cost, rougher surface, good adhesion, and is suitable for large-area flat bonding and die-cutting parts. Surface treatment determines interface reliability: bare copper can be soldered but is prone to oxidation; Tin plating improves solderability and storage stability; Nickel plating improves corrosion resistance and long-term stability of contact resistance, and is a common choice for precision grounding.

conductive adhesiveIt is formed by filling conductive particles in a pressure-sensitive adhesive matrix (acrylic or silicone rubber system). Common filler systems include nickel powder, silver powder, silver coated copper, nickel coated copper, nickel coated graphite, etc. After the filler content exceeds the percolation threshold, particles form bridges in the thickness direction, and the adhesive layer has the ability to conduct z-direction; Insufficient filler will only result in "adhesion without conductivity", while excessive filler will sacrifice initial adhesion and peel strength. This is why conductive tape is generally softer and less adhesive than structural tape of the same thickness.

First, distinguish the type of adhesiveConductive adhesive (z-conductive, used for grounding and bonding)/Insulated backing adhesive (only fixed, non-conductive)/Single sided conductive (only conductive on the copper foil surface). If you buy the wrong item, all subsequent parameters lose their meaning, and the appearance of the three is often almost the same.

02Thickness: sufficient electrically, not necessarily mechanically

The square resistance of copper is inversely proportional to its thickness, and the current at high frequencies is concentrated in the surface layer. Based on a copper resistivity of 1.72 × 10 Ω· m at 20 ℃, the theoretical resistivity and corresponding frequency skin depth for several common thicknesses are as follows:

copper thickness Theoretical resistance (Ω/□) Skin depth reference
6μm About 2.9 × 10 ⁻ ³ —
12μm About 1.4 × 10 ⁻ ³ The skin depth (about 2 μ m) at ≈ 1GHz is much smaller than this
18μm About 9.6 × 10 ⁻⁴ 3 times the skin depth (approximately 6.6 μ m) at ≈ 100MHz
35μm(1oz) About 4.9 × 10 ⁻⁴ 1.7 times the skin depth (approximately 21 μ m) at ≈ 10MHz
70μm About 2.5 × 10 ⁻⁴ Skin depth (approximately 66 μ m) at ≈ 1MHz

This table can explain a common misjudgment: in the GHz band, the reflection and shielding contributions of a copper layer of more than ten microns are already close to "sufficient"; Continuing to increase, the benefits mainly fall on mechanical strength, flexural life, current carrying capacity, and welding allowance, rather than shielding effectiveness. On the other hand, if the target frequency band is below several hundred MHz or if low-frequency magnetic fields need to be shielded, the magnetic permeability of the copper foil itself is equal to 1, and no matter how thick it is, it cannot help - that is the battlefield for high permeability materials (such as perovskite alloys, nanocrystals, and soft magnetic wave plates).

03What exactly does conductive adhesive conduct

What is the real assessment of conductive tapeZ-directional resistance penetrating the adhesive layerInstead of the copper foil's own resistance. It is composed of three parts connected in series: the interface between the copper foil and the adhesive layer, the particle bridging inside the adhesive layer, and the interface between the adhesive layer and the object being pasted. If any of the three links are broken, the entire tape will degrade into a "tightly adhered insulating copper foil".

Therefore, the bonding process is not an auxiliary step, but a part of the electrical performance. Pressure sensitive conductive adhesive requires sufficient pressure to allow the adhesive layer to flow out and particles to come into contact with the surface; Insufficient pressure, adherence to bubbles, oxidation or oil stains on the surface, and excessive rebound stress on the curved surface can all push the z-direction resistance from tens of milliohms to hundreds of milliohms or even make it impossible. The common practice in engineering is to perform plasma or solvent cleaning before bonding, use a roller to remove bubbles in one direction, specify the pressing pressure and residence time for key overlap points, and measure the contact resistance during mass production instead of just looking at the appearance.

Remember one sentenceThe shielding effect depends on the weakest section: a 1m Ω lap link will be completely invalidated by a 1M Ω insulated contact point.

04How to read key parameters

parameter Common range/caliber pronunciation
copper thickness 6–70μm(1oz≈35μm) Electrical inspection focuses on skin depth, while structural inspection focuses on durability and current carrying capacity
Adhesive layer thickness Commonly used in the range of 20-80 μ m The thicker the joint, the easier it is to fill, but the risk of z-direction resistance and edge curling increases
Z-direction resistance From tens of milliohms to hundreds of milliohms Pressure, contact area, and test surface must be specified
180 ° peel strength About 0.5-2.5 N/25mm Conductive adhesive is generally lower than structural adhesive and needs to be balanced with the risk of edge curling
heat-resistant Acrylic acid system is about -20~120 ℃; Silicone system is higher Mostly attached after assembly, not suitable for direct reflow
Flame retardant/environmentally friendly UL94 V-0、 Halogen-free RoHS/REACH Must check models near the battery, inside the casing, and exit
shielding effectiveness The common aperture of the whole machine is 40-80dB, which strongly relies on gaps and overlaps The material grade value is not equal to the result after installing the entire machine

Parameters should be viewed in groups. Pursuing extremely low z-resistance often requires a higher filler content, at the cost of reduced initial adhesion and flexibility, making it easier to warp on curved surfaces and narrow borders; Pursuing high peel strength may increase the thickness of the adhesive layer and instead raise the z-direction resistance. The truly suitable combination is always determined by the combination of veneer material, structural stress, and target frequency band.

05Common Failure: Four More Deadly Problems Than Parameters

Edge curling and rebound.The narrow strip is attached to the curved surface or corner of the shielding cover, and the adhesive layer cannot absorb the rebound stress of the structure. The edge is lifted first after high-temperature cycling, forming an antenna like gap, and leakage often occurs at this position.

Copper surface oxidation.Bare copper forms an oxide layer on its surface in storage and humid environments, and the contact resistance increases over time. For situations that require long-term stability, choose nickel plating or tin plating surface treatment, and include storage conditions and shelf life in the specifications.

Galvanic corrosion.Copper comes into direct contact with aluminum and magnesium alloys, forming the primary battery in a humid environment, with the aluminum side being preferentially corroded. When overlapping materials, nickel plated isolation layers or composite structures are required, which is the most common hidden failure in lightweight chassis projects.

Excess and residual glue.The adhesive layer flows towards the edge under pressure and temperature, contaminating adjacent solder pads and entering the connector; Incomplete cleaning of residual adhesive during repair and tearing can cause the second bonding to fail directly. The shrinkage and release design of the adhesive layer of die cut parts are designed to serve this purpose.

06Division of labor: One section each for tape, wave absorbing plate, and shielding cover

Material Typical location
Conductive adhesive copper foil tape Conductive overlap, edge sealing, local shielding Shield cover seam, FPC grounding terminal, connector and module perimeter
Flexible soft magnetic wave plate Absorb near-field noise and convert it into heat Above the chip, on the inner wall of the shielding cover, and along the FPC routing line
Shielding cover/metal shell Far field shielding and structural load-bearing Main shielding chamber of the whole machine

The three are in series relationship: the shielding cover provides most of the shielding effectiveness, the tape fills its seams with the grounding path, and the absorbing wave plate handles repeated reflections and near-field coupling inside the cavity. If any section is disconnected, the effect of the other two sections will be dragged to a very low level - this is also the most common reason for "replacing more expensive materials without improvement" in the overall machine rectification.

07Acceptance: Three numbers that must be conditional

If the data of conductive tape lacks testing conditions, it has little comparative value. At least three items should be monitored during acceptance: contact resistance (using a four point probe or milliohmmeter to specify the measuring point, pressure, and area), 180 ° peel strength (specifying the material and tensile speed of the veneer), and retested values after high temperature, high humidity, or temperature cycling. The shielding effectiveness should be measured on the entire machine or simulated cavity, and material grade values can only be used as screening references.

Three follow-up questions during procurementIs the adhesive conductive or insulating? Is the copper surface bare copper, tin plated, or nickel plated? Have the testing conditions for contact resistance been clearly stated? These three questions cannot be answered, and subsequent failure analysis is basically at a loss.

The value of copper foil tape lies not in how thick the copper is, but in a path that does not drop the chain from the copper surface to the grounding point. Designing the thickness, adhesive layer, and bonding process as a whole is the most cost-effective and effective shielding patch; Upon opening, it appears to be just three pieces of material stacked together.

For more technical information on conductive shielding materials, flexible soft magnetic absorbing materials, and precious metal pastes, please visitwww.avanzado.cn.

Contact

Contact Us

Company:Xianjin Yuan (Shenzhen) Technology Co., Ltd.

Address: 8/F, Zhongxing Building, Shajing Xinsha Road, Bao'an District, Shenzhen, Guangdong, China

Tel: 0755-22277778   13826586185

Email:duanlian@shturl.cc /YvXa