Technical Note / Process & Performance
The two suppliers provided almost identical ingredient lists: the same iron silicon aluminum powder, the same resin system, and the same filling ratio. The samples were sent to the laboratory, with one showing significant attenuation around 2.4GHz and the other only half of it; Place two pieces under a microscope to examine the cross-section, and the difference is clear at a glance - the former has layers of flake like powder that are evenly spread and oriented, while the latter is haphazardly stacked with clustered blocks in some areas.The formula determines the upper limit, and the process determines whether the upper limit can be reached.
For EMI soft magnetic absorbing materials, the real difficulty is not to "mix magnetic powder into resin", but to make each flat powder face in the same direction, insulated from each other, evenly dispersed, and controlled within micrometer level consistency in thickness. These things are all in the process.
The molding processes in the industry are basically divided into two categories. After mixing the magnetic powder with resin using a dry method, it is repeatedly rolled into sheets using a rolling roller, and the sheet shaped powder is partially oriented by shear force; The wet method mixes magnetic powder, resin, and solvent into a slurry, which is coated on a carrier film, dried, oriented by a magnetic field, and cured. The two are not in a "new old" relationship, but each has a suitable thickness range.
The trend towards thinning has pushed most of the demand towards the wet process route: only by applying a magnetic field before the wet film has solidified can the flake powder be truly stacked parallel to the surface of the sheet; Although dry shear orientation also has an effect, it is limited by viscoelasticity and it is difficult to achieve the same level of orientation. That's also why almost all products in the 25-50 μ m range come from coating processes.
Flattening degree.Ball milling or flaking process compresses powder into thin sheets, with a larger aspect ratio, thinner sheet thickness, stronger shape anisotropy, and easier resonance frequency to be pushed to high frequencies. But the thinner the thickness, the better: being too thin will reduce the filling density, increase the interface area, and instead raise the dielectric constant.
Disperse quality.Agglomeration will form high concentration areas locally, where ε 'is higher and eddy currents are intensified, resulting in a "hot spot" type of local reflection; At the same time, aggregates are mechanical weak points that crack first during bending and die-cutting. Uneven dispersion is the top reason for "different performance of the same formula".
Orientation strength and directional consistency.The orientation field applied during the wet film stage is usually on the Tesla scale, and the field strength and time together determine the degree of orientation. Good orientation results in an increase in in-plane effective magnetic permeability, enhanced out of plane demagnetization effect, and an upward shift in equivalent resonance frequency; If the orientation is inconsistent, it is manifested as the frequency response curves of the same batch of sheets at different positions being offset from each other.
Insulation coating.Each powder surface is completely wrapped in resin to maintain high filling while suppressing eddy currents and conductivity. In areas where the coating is incomplete, tiny conductive bridges are formed between particles, resulting in a decrease in surface resistance. The material gradually becomes a conductor at high frequencies, with increased reflection and decreased absorption.
Drying and solidification curve.Heating up too quickly can cause solvent residue and surface crust, preventing internal solvents from coming out and forming micropores and stress; Insufficient curing results in poor adhesion and easy precipitation during long-term use. These types of defects are often not visible during factory testing, but they tend to erupt during high temperature or humid heat tests at the client end.
The attenuation of a waveplate is approximately proportional to its thickness. This sentence becomes a cruel arithmetic problem on thin sheets: for a 0.05mm sheet, if the thickness fluctuates by ± 5 μ m, there is a performance difference of ± 10%; On a 0.2mm sheet, the same absolute fluctuation only accounts for ± 2.5%. This is why ultra-thin products require much higher coating accuracy than thick sheets, and it is also one of the reasons why the same formula produces different results on different production lines.
Thickness fluctuations can also affect performance in another way: locally thicker areas absorb lower frequency peaks, while thinner areas have higher peak positions. After the entire film is stacked, the frequency response curve is "smoothed out" - although the peak values appear to be lower, in reality, the regions are not synchronized. This type of problem cannot be solved by sticking it tighter, it can only be screened out during the incoming material stage.
The coating is only halfway done. Composite backing, release film, slitting, die-cutting, and winding packaging, each step may offset the performance of the front section. The uniformity of the backing layer affects the adhesion of bubbles and local thickness; Die cutting burrs and blade compression can cause edge powder loss and insulation degradation; Poor control of coil tension can leave invisible residual stress inside the sheet, resulting in edge warping during temperature cycling after bonding.
For customers, these later stage capabilities often determine the mass production yield more than the formula. The edge quality and powder loss rate obtained by laser die-cutting and flat knife die-cutting of the same roll of material are completely different; For ultra-thin products, it is more common to use low adhesion release films and control the unwinding tension to avoid lifting the magnetic layer together during peeling.
Remember one sentenceThe formula determines how well it can do, and the process determines whether it can do so well every time. The former is a laboratory indicator, while the latter is a mass production indicator.
You don't need to look at the promotional page, just look at the four types of data. The first category isThickness distributionRequest the measured thickness values and tolerances of multiple points on the same roll, instead of the nominal values. The second category iscross-sectional morphologyA magnified cross-sectional view can reveal whether the dispersion is uniform, whether the orientation of the flake powder is consistent, and whether the coating layer is complete.
The third category isBatch consistencyThe distribution of peak frequency and peak height for multiple batches of the same specification is more convincing than the "best data" for a single batch. The fourth category isProcess capabilityThe CpK or process control scheme for critical dimensions and parameters determines the stability of long-term supply and also determines whether to repeatedly conduct failure analysis for the "unlucky batch" in the future.
If a specification only states' μ 'peak value ≥ a certain value', process differences will be completely hidden. A more usable way is to include the process correlation in the paper: thickness tolerance and measuring points, lower limit of surface resistance, determination method of cross-sectional orientation, allowable drift range of batch frequency response, and quality criteria for die-cutting edges. These terms will not make the product better, but they will turn 'good' into reproducible results.
EMI soft magnetic absorbing material may appear as a "black sheet", but in reality, it is a process chain that extends from powder, slurry, orientation field, drying curve all the way to the die-cutting blade. Evaluating a chain is closer to real purchasing decisions than evaluating a single piece.
For more technical information on magnetic absorbing materials, shielding materials, and precious metal pastes, please visitwww.avanzado.cn.
Contact
Company:Xianjin Yuan (Shenzhen) Technology Co., Ltd.
Address: 8/F, Zhongxing Building, Shajing Xinsha Road, Bao'an District, Shenzhen, Guangdong, China
Tel: 0755-22277778 13826586185
Email: duanlian@shturl.cc /LtQc
Advanced Institute (Shenzhen) Technology Co., Ltd, © two thousand and twenty-onewww.xianjinyuan.cn. All Rights Reserved.Guangdong ICP No. 2021051947 sitemap