Frontier News

EMI Soft Magnetic Absorbing Materials: Neglected Dielectric Parameters and Impedance Matching

Time:2026-11-19Number:26

Technical Note  /  Impedance & Loss

Two EMI soft magnetic absorbing materials, in the same frequency band, the difference in μ "on the specification sheet is not significant. Installed on the same test board, A brings nearly double-digit attenuation, while B only gives a few dB. The engineer's first reaction is' B's formula doesn't work '. But a more common reason is that the dielectric constant of B is significantly higher, and most of the electromagnetic waves are reflected off the surface of the material, preventing the energy from dissipating into the material.If a 'absorbing material' bounces the wave back first, its μ 'cannot be used no matter how high it is.

This is the missing half in most selection tables: magnetic permeability determines "whether it can dissipate", and dielectric constant determines "whether it can enter". Both must be viewed together.

01Absorption requires meeting two conditions simultaneously

The first condition isGet inThe wave impedance in free space is about 377 Ω, and if the input impedance on the material surface differs greatly from it, the incident wave will be heavily reflected at the interface. The second condition isCan keep itThe energy entering the interior of the material needs to be gradually converted into heat by magnetic and dielectric losses, rather than penetrating and exiting from the other side.

For a layer of absorbing material attached to a metal backing, its input impedance is determined by the complex magnetic permeability and complex dielectric constant, which can be simplified as:

Z c= Z 0· √(μ r/ ε r)    Γ = (Z in− Z 0) / (Z inZ 0)

A often overlooked fact can be directly read from this set of equations: μrWith εrIn impedance, there is a division relationship. Only increasing the magnetic permeability while simultaneously increasing the dielectric constant may result in almost no change in the ratio, and the interface reflection may not improve or even deteriorate; On the contrary, moderately controlling ε and increasing μ actually makes it easier for energy to enter the material.

parameter Physical Role The consequences of deviation
μ′ Magnetic gathering ability determines the efficiency of magnetic flux entering the chip If it is too low, the thin film will not have enough magnetism to gather; Too high will lower the resonance frequency
μ″ Magnetic loss, converting energy into heat It is the core of absorption, but it requires energy to come in and take effect
ε′ Dielectric energy storage affects interface impedance and wavelength compression Excessive height leads to surface reflection and resonance shift; If it is too low, the thickness must be increased
ε″ Dielectric loss, with an increase in the proportion of high-frequency bands Can compensate for high-frequency magnetic loss attenuation, but if it is too large, it will cause the sheet to approach the conductor

02Where does the ε of soft magnetic absorbing materials come from

It is not an incidental parameter, but an inevitable result determined by the structure. The resin matrix itself contains polar groups, which generate dipole polarization in an alternating field; There are a large number of interfaces between metal powder and resin, and the interface polarization contributes significantly in the low-frequency range; The finer the powder and the larger the specific surface area, the stronger the interface contribution. When the filling ratio approaches the percolation threshold, small conductive pathways are formed between particles, and ε 'will rapidly increase. At the same time, the conductivity will increase, and eddy currents and reflections will intensify together.

This also explains why the practice of "adding filling to mention μ" has a ceiling: as the filling increases, the ε and conductivity increase synchronously, and the material gradually changes from a "magnetic absorber" to a "lossy conductor", with enhanced surface reflection and reduced internal dissipation. The high filling formula in engineering often requires insulation coating and dispersion processes to suppress this upward curve.

03High frequency range: The proportion of dielectric loss is changing

In near-field applications ranging from hundreds of MHz to several GHz, magnetic losses are usually the main contributor, which is why composite absorbing materials are called "magnetic absorbing". But as the frequency continues to increase, the magnetic loss decreases due to resonance, and the relative share of dielectric loss, radiation, and substrate loss increases. In the millimeter wave band, the attenuation of many materials is no longer solely dominated by μ ", and the weight of ε" and structural loss is significantly increased.

The direct significance of selection is that the high-frequency performance cannot be inferred from the measured μ "in the low-frequency range, nor can the variation of ε" with frequency be ignored. When evaluating high-frequency applications, it is necessary to request four curves covering the target frequency band (μ ′, μ ″, ε′, ε″), rather than a set of single point values.

Remember one sentenceμ "determines whether it can dissipate, while ε determines whether it can enter. The specification sheet for reporting only μ "only tells half of the story.

04Thickness: It's not the thicker the better, it's a matching issue

Thickness is involved in two mechanisms: impedance and phase. On the one hand, an increase in thickness will change the input impedance, causing a decrease in surface reflection and allowing more energy to enter; On the other hand, changes in the electrical length inside the material can cause interference effects, resulting in absorption peaks at specific frequencies. That's why the same formula will have different peak frequencies at different thicknesses - it's not 'performance getting better or worse', but rather the matching point moving.

Therefore, using "thickening" to save a wrongly selected formula usually only involves shifting the peak position elsewhere. The correct sequence is to first confirm whether the material's μ and ε in the target frequency band are suitable, then adjust the matching point with thickness, and finally confirm the result with measured attenuation.

05Inherent blind spots in reflection method testing

The "absorption" curve provided in many specifications is the reflection loss measured using the metal backing method. This curve only reflects' how much energy has not returned to the incident direction ', itSurface reflectionandInternal absorptionMerge into one number. So there is a misconception: a material with a high ε and almost total reflection may appear to have a "deep" curve, but it actually does not absorb any energy.

To distinguish between the two, the transmission line method or free space method should be used, and S11 and S21 should be read at the same time to calculate the true dissipation ratio according to power conservation:Ploss/Pin = 1 − |S11|² − |S21|²For EMI suppression, this is the direct evidence of how much has been absorbed.

Ask four questions when requesting dataIs it measuring reflection loss or transmission loss? What are fixtures and line widths? Does the sample contain adhesive layer and insulation film? Are μ and ε eigenvalues or equivalent values? After completing the four questions and answers, the two curves can be compared.

06There is also a ripple effect: it will change your circuit as well

The increase in ε will compress the wavelength inside the material, and the change in equivalent dielectric constant will alter the characteristic impedance and propagation delay of adjacent traces. Attaching the absorbing wave plate near the high-speed differential line may not only reduce noise, but also result in impedance discontinuity and eye diagram changes; If it is placed near the antenna, it will shift the resonant frequency. These are not 'side effects', but rather the manifestation of the same set of electromagnetic parameters in another location.

So a complete validation should include two types of results: the noise side (attenuation at the target frequency) and the signal side (insertion loss, impedance, eye diagram/bit error rate, or antenna efficiency). Only testing the former can easily shift the problem from radiation to signal integrity.

07Material selection list

Need to request Usage
Frequency response curves of μ 'and μ' Determine whether the peak position is aligned with the target frequency band and whether the magnetic gathering ability is sufficient
Frequency response curves of ε′ and ε″ Assessing the risk of interface reflection and the contribution of high-frequency dielectric loss
Surface/Volume Resistance Determine whether it is possible to directly attach bare wires and whether there is a risk of leakage and short circuit
Power loss measured curve Including fixtures, distance, and sample size, directly corresponding to actual suppression capability
Thickness and total thickness Distinguish between magnetic layer and adhesive layer to avoid misestimation of stacking space

The selection of EMI soft magnetic absorbing materials is essentially about finding balance on a complex plane: magnetic losses provide dissipation capability, dielectric constant determines whether energy can enter the field, and thickness is responsible for adjusting the two to the matching point. Putting these three together, many phenomena of "the same specification but different effects" will become explainable.

For more technical information on magnetic absorbing materials, shielding materials, and precious metal pastes, please visitwww.avanzado.cn.

Contact

Contact Us

Company:Xianjin Yuan (Shenzhen) Technology Co., Ltd.

Address: 8/F, Zhongxing Building, Shajing Xinsha Road, Bao'an District, Shenzhen, Guangdong, China

Tel: 0755-22277778   13826586185

Email: duanlian@shturl.cc /Iclw

Hotline
0755-22277778
13826586185(Mr.Duan)
Wechat QRcode Wechat QRcode