Frontier News

Air gap effect: why the high magnetic permeability of ferrite absorbing wave plates cannot be attached

Time:2026-11-20Number:33

Technical Note  /  Effective Permeability

The same ferrite absorber plate has a specification of 200 μ '. Project A has been posted, and the NFC reading distance has been improved; Project B uses the same sheet and position, with almost no change in reading distance. Upon opening, the difference is minimal: A uses a 20 μ m thin adhesive and is pressed together, while B uses a 50 μ m thick adhesive. Additionally, due to slight warping of the sheet, there is an invisible gap in the middle.High magnetic permeability is not a property of materials, but a property of "material+interface".

In the magnetic circuit, air gap is the most expensive thing. It doesn't need to be very wide - just a few tens of micrometers is enough to cut a permeability of 200 to below 100.

01First, calculate how much magnetic permeability can be consumed by the air gap

Simplify the magnetic circuit into a series model of "magnetic layer+air gap", and the effective magnetic permeability can be approximated as:

μ eff= μ r/ ( 1 μ r· l g/ l e)

Among them, lgFor the total thickness of the air gap, leThe effective magnetic path length of the magnetic layer. The key is the product in the denominator: μrThe higher, the greater the amplification factor of the air gap. in other wordsMaterials with higher magnetic permeability are less able to withstand air gaps.

Proportion of air gap to magnetic circuit μr=At 100 hourseff μr=At 200 hourseff
0.1% About 91 About 167
0.5% About 67 About 100
1% About 50 About 67
2% About 33 About 40
5% About 17 About 18

Placing it in a real structure is more intuitive: a 0.1mm thick piece of ferrite, if there is a 10 μ m air gap in between, the air gap accounts for 10%; Considering the adhesive layer and surface roughness, this number is not uncommon in mass production. That's also why "changing to a higher μ 'material" often has no effect - μrFrom 200 to 300, the air gap also increased from 1% to 2%, almost offsetting each other.

02Five sources of air gap

The backing layer itself.This is the most easily overlooked type: glue is not a magnetic medium, itsr≈ 1, equivalent to an air gap in the magnetic circuit. A 50 μ m adhesive is attached behind a 0.1mm magnetic sheet, with an air gap ratio of over 30%. Choosing thin adhesive and high filling magnetic adhesive is the only effective solution here.

Surface roughness and flatness.Even after grinding, there are still microscopic undulations on the surface of sintered ferrite; Flexible composite sheets may also exhibit ripples after curing. When two rough surfaces are in contact, the actual contact area only accounts for a part, and the non-contact area is the air gap.

Warping and local voids.The sintered sheet will slightly warp under sintering shrinkage and stacking stress, and only partially make real contact after being attached to a large plane, while the rest of the area is suspended by the adhesive layer. This type of air gap distribution is uneven, and it is measured that the overall effective magnetic permeability is low and unstable.

Fit pressure and process.Manual attachment is difficult to ensure uniform pressure; If the roller direction is single in automated bonding, bubbles will be pushed to one side to form strip-shaped gaps. When the compression is insufficient, the actual thickness of the adhesive layer is thicker than the nominal value, which is equivalent to artificially increasing the air gap.

Thermal and structural deformation.The difference in thermal expansion coefficients of different materials causes micro gaps to reappear at the originally tightly adhered interface after temperature cycling; Uneven tightening of screws can cause local stress concentration, leading to delamination after long-term operation.

Remember one sentenceIn the magnetic circuit, the adhesive layer is the air gap. You didn't choose 'adhesive backing', you chose a section of magnetic resistance.

03What has it done for the three indicators it is correct for

In the NFC and RFID scenarios, the decrease in effective magnetic permeability is directly reflected in low coil inductance, changes in Q value, and thus shortened reading distance. The reading distance has a strong dependence on magnetic permeability, but it is not nonlinear - when the magnetic flux is already largely cancelled out by the metal, any point of magnetic permeability loss will be amplified.

In wireless charging scenarios, the air gap can cause a decrease in coupling coefficient, efficiency, and may allow the coil to enter saturation earlier at high currents. Due to the working frequency in the hundreds of kHz range, the wavelength is long and the tolerance of the air gap is relatively loose. However, the magnetic flux density here is high, and saturation issues are more worthy of attention than magnetic permeability losses.

In the scenario of low-frequency suppression and magnetic circuit shielding, μeffThe decrease means that the magnetic flux is more likely to bypass the material and take the air path - both shielding and guidance fail simultaneously. These types of applications often use the three actions of "close, full, and tight" to ensure effectiveness, essentially compressing the air gap.

04Who is more afraid of air gaps between sintered sheets and flexible sheets

dimension Sintered ferrite sheet Flexible composite sheet
μrstarting point High, therefore highly sensitive to air gaps Lower, relatively better tolerance
Deformation adaptability Poor, difficult to eliminate warping and roughness Okay, it can absorb tolerances and surfaces
risk point Cracking, partial suspension μeffSignificantly lower than the nominal value μrIt is inherently low and requires a larger compensation area
Applicable conclusion Flat, pressurized, and tolerance controlled structure Structures with curved surfaces, thin walls, and large tolerances

This table explains a counterintuitive phenomenon: some projects switch to using μrThe higher the sintered sheet, the worse the effect, because it amplifies the amplification effect of the air gap. The μ of flexible sheetrAlthough it is only half, the μ on the real interfaceeffPerhaps even higher.

05How to lower the air gap

Choose glue before choosing film.Write the thickness of the adhesive layer into the specifications, giving priority to thin adhesive or high filling magnetic conductive adhesive; If the structure allows, use compression or embedding instead of pure adhesive tape to directly press the metal or structural components against the magnetic sheet.

Control the flatness.Propose an upper limit for the warpage of sintered sheets and conduct random inspections upon receipt of materials; For large-sized sheets, it is better to divide them into multiple pieces and splice them together than to leave the entire piece hanging.

Set parameters for the process.Specify the pressing pressure, roller direction, and bonding speed to make the "tight" action reproducible; Perform cross-sectional sectioning or ultrasonic examination on key positions after bonding to confirm that there are no continuous gaps.

Using μeffAcceptance, not μr.Measuring the effective magnetic permeability using inductance or magnetic circuit methods in the finished product state can better reflect the true performance than measuring the eigenvalues on the sample. This is also the most direct way to determine whether there is a problem with the material or assembly.

06A cascading effect that is easily overlooked

The air gap not only reduces the magnetic permeability, but also changes the saturation behavior and temperature rise distribution of the magnetic circuit. Due to the magnetic flux being squeezed into the actual contact area, the local magnetic flux density increases, making it easier for the material to saturate at the contact edge first; At the same time, the adhesive layer in the non-contact area bears more thermal resistance, forming a temperature gradient. In terms of performance, it is' the same piece of material, where it comes into contact, heats up first and saturates first ', rather than working uniformly as a whole.

The technical content of ferrite absorbing plates is half in the formula and the other half at the interface. Design the adhesive layer as a section of the magnetic circuit and the bonding as a process, only then will the nominal permeability of 200 have a chance to truly appear in your reading distance and efficiency.

For more technical information on ferrite absorbing materials, flexible soft magnetic absorbing materials, and conductive shielding materials, please visitwww.avanzado.cn.

Contact

Contact Us

Company:Xianjin Yuan (Shenzhen) Technology Co., Ltd.

Address: 8/F, Zhongxing Building, Shajing Xinsha Road, Bao'an District, Shenzhen, Guangdong, China

Tel: 0755-22277778   13826586185

Email: duanlian@shturl.cc /doFr

Hotline
0755-22277778
13826586185(Mr.Duan)
Wechat QRcode Wechat QRcode