Frontier News

How much dB can strong adhesive copper foil tape block: triple limitations of thickness, gap, and overlap

Time:2026-11-20Number:33

Technical Note  /  Shielding Effectiveness

The same roll of strong adhesive copper foil tape has a high shielding value measured on the flange coaxial fixture in the materials laboratory, and the specification sheet looks impeccable. When installed on the entire machine and tested again, the effective shielding is only 20-30 decibels, and there are occasional spikes.The difference is not in copper foil, but in the gap between "material level" and "assembly level": the former measures copper, while the latter measures seams.

To determine the effectiveness of a piece of tape in your product, it is necessary to calculate three layers of limitations: how much material can be provided, how much geometry allows for retention, and how much overlap can be conducted.

01Shielding consists of three components, with thin film metal primarily reflecting

The shielding effectiveness is usually divided into three parts: reflection, absorption, and multiple reflections. For highly conductive and non-magnetic thin film materials such as copper, the magnetic permeability is equal to 1, and there is almost no magnetic loss. The shielding almost entirely comes from "reflection caused by impedance mismatch" and "small absorption after entering". This also means that it has an impact onElectric fields and plane waves are effective, but almost ineffective against low-frequency magnetic fields——The latter requires high magnetic permeability materials for magnetic flux diversion.

The strength of the absorption term is determined by the ratio of thickness to skin depth. According to simplified estimation, the absorption attenuation (dB) is roughly proportional to t/δ, where δ is the skin depth of copper at that frequency.

A(dB) ≈ 8.686 · t / δ
frequency Skin depth of copper Absorption attenuation of 35 μ m copper foil (estimated)
1MHz About 66 μ m About 5dB
10MHz About 21 μ m About 15dB
100MHz About 6.6 μ m About 46dB
1GHz About 2.1 μ m About 145dB (far beyond actual)
10GHz About 0.66 μ m The thickness has far exceeded the required amount

The most important information in this table is not the values themselves, but a conclusion:Above 100MHz, the material margin of 35 μ m copper foil is already extremely abundant, and choosing thicker copper foil has almost no help for shielding.The thickness should be determined by mechanical strength, flexural life, current carrying capacity, and welding requirements, rather than by "wanting to shield more". On the contrary, at the 1MHz level, the absorption of thin film copper is only in the single digit dB, and it is unrealistic to expect it to solve low-frequency problems.

02Second layer: Geometry brings theoretical limits back to reality

There is almost no "fully coated copper" in real products. Tape is applied in sections, with seams, overlapping edges, corners, and openings all weakening the shielding. The radiation efficiency of the gap is determined by itsMaximum sizeDecided to become a resonant radiator when approaching half a wavelength; Therefore, the control objective is not "how wide the seam is", but "how long is the longest section".

The treatment methods for holes and gaps are different. The leakage of a single small hole varies rapidly with the ratio of aperture to wavelength, while the leakage of a hole array is related to the aperture ratio; A row of dense small holes is often gentler than a narrow slit of the same length. This is also the reason why ventilation and heat dissipation openings are often made into array holes instead of long slits.

Therefore, using a strong adhesive copper foil tape to "fill" a 10cm gap, if not segmented, the actual result may only be replacing one resonant gap with two - rather than increasing the shielding value by 40dB. The benefits at the geometric level always take precedence over the material level reinforcement.

Remember one sentenceMaterials determine the upper limit, geometry determines the actual value. The 20-30 dB measured on the whole machine are almost all answers written in geometry.

03Third layer: Overlapping impedance and common mode path

No matter how good the copper foil itself is, if there is only a non-conductive layer of adhesive or a long and narrow overlap between it and the reference ground, the shielding cavity is just a "suspended copper skin". At low frequencies, look at resistance; at high frequencies, look at inductance: a long and narrow overlap at high frequencies presents high impedance, which is equivalent to no connection.

This is also a concrete manifestation of the contradiction between strong adhesion and grounding. Strong adhesive formulas usually have softer adhesive layers and thicker coatings, and the contact between conductive particles is not as stable as the conductive adhesive type of thin adhesive; If this tape needs to be both firmly adhered and conductive, the z-direction resistance must be separately specified and measured, and it cannot be assumed that 'good copper foil means good grounding'.

04Two tests, two worlds

test method What is being tested Why are the results different
Coaxial/flange fixture The plane wave shielding effectiveness of the material itself No gaps or overlaps, approaching the theoretical upper limit of the material
Shielding room/whole machine Actual leakage in assembly state All gaps, overlaps, cables, and common mode paths are included
Near field scanning Hot spot location and leakage distribution Used for positioning, not for providing a single numerical value

These three methods are not interchangeable, but answer three different questions: whether the materials are sufficient, whether the assembly is leaking, and where the leaks are. If only comparing material grade numbers in procurement negotiations, it is easy to choose the one that is "the strongest on paper and the weakest on paper".

05Apply the tape to four actions close to the theoretical upper limit

Continuous coverage without leaving long gaps.It is better to use multiple segments for splicing than to let the length of any segment approach half a wavelength; Diagonal stacking at the corner to avoid uneven adhesive layer after right angle stretching.

Grounding nearby and parallel connection of multiple points.Distribute the grounding points of the tape to every edge instead of pulling diagonally from one corner; The spacing between overlapping points is controlled at the level of λ/20 of the highest attention frequency.

Compact first, then talk about shielding.Insufficient compression will simultaneously destroy the adhesion and contact: the adhesive layer has not flowed out, the z-direction resistance is high, and gaps still exist. The compression parameters should be included in the homework guide rather than relying on the feel.

Select surface treatment according to the environment.Bare copper is prone to oxidation, and nickel plating is preferred for long-term grounding applications; Choose tin plated surface when welding is required. The impact of surface treatment is on 'how much shielding remains in the long term', rather than 'how high it was at the time of leaving the factory'.

06The correct sequence of questions when selecting

First, ask about the frequency: whether the target frequency band is within the effective range of thin film copper (about 100 MHz or above). If it is a low-frequency magnetic field, replace the material directly instead of thickening it. Ask geometry again: how much can the longest gap be controlled, and whether segmentation and padding are needed. Then ask the system if the grounding path is nearby and if there are multiple points. Finally, I asked about the thickness and surface treatment of the copper foil - it answered about mechanical, corrosion resistance, and welding, not shielding.

The true boundary of the ability of strong adhesive copper foil tape is not how thick its copper is, but whether you stick it into a complete piece of copper or a string of small pieces cut by gaps. Taking into account all three restrictions, that tape will give you the actual number you need on the entire machine.

For more technical information on conductive shielding materials, copper foil tapes, and flexible soft magnetic absorbing materials, please visitwww.avanzado.cn.

Contact

Contact Us

Company:Xianjin Yuan (Shenzhen) Technology Co., Ltd.

Address: 8/F, Zhongxing Building, Shajing Xinsha Road, Bao'an District, Shenzhen, Guangdong, China

Tel: 0755-22277778   13826586185

Email: duanlian@shturl.cc /Gz8L

Hotline
0755-22277778
13826586185(Mr.Duan)