Compression of soft magnetic composite materials: uneven density is more likely to destroy consistency than formula

Time:2026-11-26Number:16

Technical Note  /  Compaction & Consistency

The same batch of soft magnetic composite material powder, the same formula, and the same press machine are used to make pressed blanks. After cutting and sampling, the magnetic permeability energy difference between the center and the edge is more than 10%, and the loss curve does not overlap. Purchasing may suspect there is a problem with the powder, and formula engineers may suspect uneven mixing.But in soft magnetic composite materials, the most common culprit is the density gradient during the compression process——The friction force experienced by the powder during compaction in the mold cavity is not uniform, resulting in a "density topographic map" inside the compact.

Density is crucial in SMC because it directly determines how much magnetic material is present per unit volume.

01Three stages, each with its own pitfalls

stage Key risks consequence
fill Poor powder flowability, bridging, and partial incomplete filling Local density is low, forming pores and weak areas
Compression Friction on the mold wall causes pressure to attenuate in the direction of compression Uneven density between top and bottom, inside and outside, and local crushing of the coating layer
demolding Rebound, demolding friction, stress concentration Layering, microcracks, dimensional deviations, and subsequent cracking

The mechanism of the second stage is worth exploring: when the pressure applied by the press is transmitted deep into the mold cavity, it will be continuously consumed by the friction between the powder and the mold wall. The higher and more complex the shape of the billet, the more pronounced the attenuation. The result is that the density at the upper end is higher than that at the lower end, and the density near the mold wall is lower than that at the center. So for the same billet, the magnetic permeability measured naturally varies depending on the sampling location.

This also explains why "thin sheets" often have better consistency than "high columns": the path in the direction of compression is shorter, and the stroke of pressure attenuation is also shorter. For products with a high aspect ratio, density gradients are almost unavoidable and can only be alleviated through technological means.

02How does density transfer to magnetic properties

parameter Change with density sensitivity
Effective magnetic permeability Rising along with it, but the growth gradually slows down High, a few percentage points of density can cause significant differences
Saturated magnetic flux Approximately linearly increasing with the volume fraction of magnetic phase In the middle, it directly affects the anti saturation ability under high current
eddy current loss When the density is too high, the coating is easily crushed, and the loss actually increases Bidirectional, there is an optimal point
mechanical strength As density increases, but brittleness increases when it is too high Directly related to demolding cracks

The third line is a unique phenomenon of SMC: blindly pursuing high density will backfire. The thickness of the coating layer is only a few tens of nanometers. When the compression pressure is too high, the insulation on the surface of the particles is squeezed and pierced, forming local conduction between particles and significantly increasing eddy current losses. Therefore, density is not necessarily 'higher, better', but rather there exists an optimal range that matches the coating process.

Key points of the projectDensity is both a performance knob and an insulation killer in SMC. Find the best point, not the highest point.

03Demoulding rebound and mold wear: invisible batch drift

At the moment of demolding, the pressed parts will experience elastic rebound, slightly increase in size, and redistribute internal stress. If the rebound is uneven, it is easy to form microcracks at the location with the highest density gradient - these cracks only propagate during subsequent annealing or assembly, becoming a source of "failure after a period of time".

Mold wear is another type of chronic drift. The size of the mold cavity changes slowly with production, and the distribution of pressing pressure changes accordingly, with density and size shifting synchronously. This drift usually accumulates on a weekly or even monthly basis, manifested as' the same production line, products from a few months ago are different from what they are now ', while all process parameters appear unchanged.

The solution is not to encrypt the inspection, but to incorporate the mold life and key dimensions into the process management: regularly measuring the mold cavity size, recording the compression pressure curve, and keeping samples for magnetic performance retesting according to batches. In contrast, only measuring the magnetic permeability of the finished product often takes until the drift is significant before it is discovered.

04The dilemma of annealing

The compression process will leave residual stress inside the particles, increasing hysteresis losses. Annealing can release stress, but the upper temperature limit is constrained by the temperature resistance of the coating layer: insufficient temperature leads to insufficient stress release; Excessive temperature can cause decomposition or failure of the coating layer, leading to a sudden increase in eddy current losses.

This window is usually very narrow, and the actual process temperature is often lower than the theoretical temperature resistance of the coating material to ensure batch stability. The result of this is that the hysteresis loss of SMC is difficult to reduce very low - this is an inherent constraint of the material system, not a problem of process level.

05How to verify consistency

item method What can be discovered
1 Geometric method for measuring density (volume and weight) Is the overall density within the window
2 Multi point sampling for measuring magnetic permeability (center, edge, top and bottom) The severity of density gradient
3 Comparison of loss curves in the mid to high frequency range Is the coating locally crushed
4 Record the compression pressure curve and mold cavity size Mold wear and batch drift
5 Sampling for appearance and crack inspection after demolding Hidden defects caused by rebound

The consistency of soft magnetic composite materials depends less on the formula and more on the uneven pressing of the powder during the few minutes of compression. Incorporating density distribution, mold state, and annealing window into process management is easier to achieve stable output than repeatedly adjusting powder formulations.

For more technical information on soft magnetic composite materials, magnetic material forming processes, and consistency control, please visitwww.avanzado.cn.

Contact

Contact us

Company:Xianjin Yuan (Shenzhen) Technology Co., Ltd.

Address: 8/F, Zhongxing Building, Shajing Xinsha Road, Bao'an District, Shenzhen, Guangdong, China

Tel: 0755-22277778   13826586185

Email: duanlian@xianjinyuan.cn

Hotline
0755-22277778
13826586185(Mr.Duan)
Wechat QRcode Wechat QRcode