Technical Note / Transmission-Line Model
The data on hand is an absorption curve with a thickness of 0.1mm, while the structure requires 0.3mm; or the supplier measures free space, but you need to stick a metal casing. Many teams spent several weeks making new samples and sending them for testing at this time.In fact, as long as we get the four variable quantities of μ ', μ ″, ε' and ε ″ with frequency, we can calculate the performance under any thickness and any backplane conditions first - thin lossy medium is essentially a transmission line.
This model is not new, but the prerequisite for using it is to correct both the input variables and boundary conditions.
The calculation chain is divided into three sections, each of which can be manually calculated or written into a spreadsheet tool.
The first paragraph is about characteristic impedance.Free space wave impedance Z0Normalized as a benchmark:
The second paragraph is about the propagation constant.It contains two parts: attenuation and phase, which determine how the wave attenuates and shifts in phase within the layer
The third paragraph is about input impedance.The metal backplate is equivalent to a terminal short circuit (with zero terminal impedance), and the input impedance on the surface of the layer is:
With ZinThe reflection coefficient and absorption rate can be directly calculated:
The value of this equation lies in the fact that thickness d is the only variable that needs to be replaced. If the four electromagnetic parameters remain unchanged, changing to'd 'will result in the entire new curve.
This is the most common misjudgment when using this type of model. There is no transmission under the metal backplate, and all incident energy ultimately has only two directions: reflection or dissipation within the layer. Therefore, theoretically, A=1 − | ∧ | ² does hold, the lower the reflection, the more absorption.
The problem lies in the physical origin of the point with the lowest reflection. It may come from two completely different mechanisms: one is that energy is indeed dissipated within the layer; The second is that the input impedance of the layer is exactly close to the free space impedance, and the wave enters smoothly but forms a standing wave inside. The energy oscillates back and forth within the layer, and eventually a considerable portion still returns. The latter will also give a very low | Gamma | under certain thickness and frequency combinations, but the intra layer field strength is very high, and a slight deviation from the design frequency will quickly deteriorate.
The discrimination method is to look at the shape of the curve: the absorption valley dominated by dissipation is usually wider, deepens and gradually widens with increasing thickness; The valley dominated by interference is usually very narrow, and the thickness adjustment disappears. What we hope to achieve in engineering is the former - it is more stable under temperature drift, thickness tolerance, and frequency offset.
Key points of the projectScan the thickness with the model and then check the width of the valley: wide and deep valleys are caused by losses, while narrow and deep valleys are caused by interference.
The phenomenon in the second line is worth mentioning: when ε 'is significantly higher than μ', the impedance mismatch between the layer surface and free space will take effect before the loss. Continuing to thicken at this point will only dissipate a little more within the layer, and there will be almost no change from the outside. Many experiences of 'adding thickness without improvement' are actually stuck in impedance rather than thickness.
For near-field EMI suppression, the values provided by the model can only be used as upper bounds for reference: the near-field source is not a plane wave, and the magnetic and electric field components are not in a fixed proportion. Actual measurements often deviate from calculations. Nevertheless, the model is still the most cost-effective first step - it can turn the question of whether the thickness value is worth doing into a matter of seconds before making a sample.
For more information on the parameters, models, and design methods of magnetic absorbing materials, please visitwww.avanzado.cn.
Contact
Company:Xianjin Yuan (Shenzhen) Technology Co., Ltd.
Address: 8/F, Zhongxing Building, Shajing Xinsha Road, Bao'an District, Shenzhen, Guangdong, China
Tel: 0755-22277778 13826586185
Email: duanlian@xianjinyuan.cn
Advanced Institute (Shenzhen) Technology Co., Ltd, © two thousand and twenty-onewww.xianjinyuan.cn. All Rights Reserved.Guangdong ICP No. 2021051947 sitemap