Technical Note / Manufacturability
The absorption curve measured by laboratory slicing of the same roll of flexible absorbing material is beautiful, but after mass production assembly, it performs averagely in overall testing. Tracing back, the problem often lies in the middle stage of the process that no one is paying close attention to:The die-cutting direction is 90 degrees wrong, bubbles are squeezed out during bonding, and the edges are thinned by the die.There is no problem with the material itself, but the process from roll to piece has lost its performance.
This paragraph is worth examining separately as it is simultaneously constrained by material properties, mold, and production line rhythm.
Flexible wave absorbing plates are mostly made of anisotropic materials, and the orientation direction determines the in-plane magnetic permeability; At the same time, it is a soft sheet material, and its thickness and flatness have a significant impact on the bonding quality. These two points must be clearly defined during the coil stage, otherwise subsequent processes cannot remedy them.
Among these items, orientation direction is the easiest to omit and also the most expensive. Most flexible wave absorbing plates have a significant difference in magnetic permeability between in-plane and out of plane, and their appearance is completely normal when the direction is cut off, which can only be exposed through actual measurements. The common practice in engineering is to make directional markings on the end of the roll and each section of release paper, and draw material grain arrows in the die-cutting drawing.
The flexible wave absorbing plate contains a high proportion of magnetic powder, with a soft texture and some rebound. When the blade is cut in, the edge will be squeezed instead of cleanly cut, forming a commonly known "collapsed edge": the thickness of the edge is lower than that of the center, and the local magnetic properties will also decrease accordingly. For smaller sheet materials, the proportion of collapsed edges may be quite significant.
Three feasible directions: First, relax the tolerance to a level that the material can stably achieve (commonly ± 0.1-0.2mm, depending on size and thickness), and do not blindly copy the accuracy of metal parts; The second is to avoid sharp inner angles and extremely narrow thin strips, which are most prone to deformation during die cutting; The third option is to switch to laser or ultrasonic cutting when necessary, in exchange for edge quality with minimal thermal impact, but to evaluate the effect of the heat affected zone on magnetic properties.
Key points of the projectThe tolerance of flexible wave absorbing plates should be given based on "soft composite materials" rather than structural components. Tight tolerances will not improve accuracy, but only increase the scrap rate.
The goal of the bonding process is only one: to ensure that there is no residual air between the sheet and the substrate. For magnetic loss materials, the air layer is non-magnetic, which means that a high resistance medium is connected in the magnetic circuit. The higher the magnetic permeability, the greater the loss. Macroscopically, we see a small bubble, while electromagnetically, we see a failure zone.
There is another variable often overlooked on automated production lines: beat. After bonding soft materials, it takes a certain amount of time for the pressure-sensitive adhesive to establish initial and final bonding strength. If the next step is immediately pulled, the interface will be damaged before curing, forming a layer that is invisible to the naked eye. For high-speed production lines, it should be confirmed whether the initial adhesion establishment time of the adhesive matches the rhythm.
In actual products, absorption plates rarely exist alone. It may be sandwiched between the shielding cover and the chip, forming a stack with copper foil, thermal pad, and insulation film. At this point, two things need to be noted.
One is the sequence. If the copper foil is placed on the outside of the absorbing plate, the magnetic flux will be reflected by the conductive layer first, reducing the chance of the absorbing plate actually participating; If the absorbing plate is placed near the heat source side, it is necessary to evaluate whether the low thermal conductivity of the absorbing plate exacerbates the local temperature rise.
The second is the total thickness and space. The effective absorption of the absorbing plate itself is related to its thickness, but each newly added layer interface in the stack may be a source of air gap. In experience, it is better to reduce the number of layers and increase the thickness of a single layer than to stack multiple thin layers with the same thickness - the more interfaces there are, the more obvious the accumulation of air gaps and uncertainties.
The technical content of flexible absorbing materials is half in the formula and the other half in delivering the original formula into the structure. Direction identification, tolerance setting, exhaust sequence, stacking sequence, storage conditions - these seemingly unrelated details actually determine whether the curve on the parameter table can be measured in the end.
For more information on die-cutting, bonding, and stacking applications of flexible absorbing materials, please visitwww.avanzado.cn.
Contact
Company:Xianjin Yuan (Shenzhen) Technology Co., Ltd.
Address: 8/F, Zhongxing Building, Shajing Xinsha Road, Bao'an District, Shenzhen, Guangdong, China
Tel: 0755 - 22277778 13826586185
Email: duanlian@xianjinyuan.cn
Advanced Institute (Shenzhen) Technology Co., Ltd, © two thousand and twenty-onewww.xianjinyuan.cn. All Rights Reserved.Guangdong ICP No. 2021051947 sitemap