Our main products include flexible substrate coating, shielding materials, absorbing materials, precious metal slurries, and more!

banner
Current:Home >Company news >Frontier News >Soft magnetic composite material: One layer of insulation coating determines how high frequency it can be used
先进院(深圳)科技有限公司

Hotline:0755-22277778 Tel:0755-22277778 
Mobile:13826586185(Mr.Duan)
Fax:0755-22277776
E-mail:duanlian@xianjinyuan.cn

Frontier News

Soft magnetic composite material: One layer of insulation coating determines how high frequency it can be used

Time:2026-11-26Number:19

Technical Note  /  Soft Magnetic Composites

The relative magnetic permeability of pure iron can easily exceed several thousand, with a saturation magnetic flux density close to 2T; while soft magnetic composite materials (SMC) made of iron powder often have a magnetic permeability of only a few tens and a reduced saturation magnetic flux. It may seem like a 'step back', but in reality it's a deliberate choice:Coating the surface of each powder with an insulation layer several tens of nanometers thick to confine eddy currents within the particles allows the material to continue working in the frequency range of tens of kHz or even MHz.The invisible coating is the core technology of SMC.

Understanding this trade-off is more important than remembering any single parameter.

01Structure: Three piece set of powder, coating, and voids

The typical process route of SMC is: coating the surface of the powder with an insulating layer → mixing with a small amount of binder → molding by compression molding → curing or low-temperature annealing. The final material consists of three parts: magnetic particles, insulation layer on the surface of the particles, and inevitable gaps and binders between the particles.

These three parts are each responsible for one thing: magnetic particles provide magnetic flux carrying capacity; The insulation layer cuts off the conductive path between particles; The gap and adhesive determine the mechanical strength, while diluting the magnetic properties. The macroscopic parameters of materials are essentially the weighted result of these three factors.

Structural elements Obtained when increasing Simultaneously losing
Fill density Effective magnetic permeability and saturation magnetic flux increase Reduced gaps, insulation layer easily crushed, and increased risk of eddy currents
Coating thickness Improved insulation and reduced high-frequency losses Magnetic permeability decreases (non-magnetic phase proportion increases)
particle size Large particle compression has high density and high magnetic permeability The eddy current path becomes longer, and the high-frequency loss increases

The relationship between the three is mutual restraint rather than simultaneous optimization. To increase magnetic permeability, one must increase density or increase particle size, which will weaken high-frequency performance; To improve high-frequency characteristics, it is necessary to thicken the coating or reduce the particles, resulting in a decrease in magnetic permeability. The formula space of SMC is essentially positioned between these three directions.

Remember one sentenceThe low magnetic permeability of SMC is not a defect, as it exchanges magnetic permeability for frequency.

02Four types of soft magnetic materials together

Material μ - level Bs level Applicable frequency band limitation
silicon steel Thousands or more About 1.8-2.0T Power frequency to several hundred Hz Stacked structure, high frequency eddy current loss
Ferrite Hundreds to thousands About 0.35-0.45T From tens of kHz to hundreds of MHz Low saturation magnetic flux, high current easily saturates
Amorphous/nanocrystalline tall About 1.2-1.4T From tens of kHz to several MHz Thin strip form, low degree of freedom in molding
Soft magnetic composite materials Dozens (commonly 20-100) About 1.0-1.6T (effective value) From tens of kHz to several MHz Low magnetic permeability, limited compression density

The values in the table are typical orders of magnitude, and the actual products vary greatly due to differences in formula and process. The significance of comparison lies in understanding their respective positions: silicon steel excels in saturated magnetic flux, ferrite excels in high frequency and low cost, nanocrystals excel in comprehensive balance, and SMC excels in shape freedom and three-dimensional magnetic circuit.

It is worth noting that although the magnetic permeability of SMC is only a few tens, it does not win by magnetic permeability. In the design of power inductors, the energy storage capacity depends on the saturation flux and volume, rather than the magnetic permeability; Magnetic permeability only affects the number of turns required to achieve the same inductance. This means that SMC is more suitable in situations where high current, small volume, and shape freedom are required.

03Three dimensional magnetic circuit: the true difference point of SMC

Silicon steel must be made into laminations, and magnetic flux can only flow along the plane of the laminations; Ferrites and nanocrystals are often in standard shapes such as rings and E-shapes. SMC is a pressed component, and magnetic flux can freely pass through in three directions, which transforms the design from "two-dimensional" to "three-dimensional".

The most direct benefit is the distributed air gap. Traditional inductors require a concentrated air gap in the magnetic circuit to prevent saturation, and the scattered magnetism at the edge of the air gap can cause additional losses and local heating; SMC disperses air gaps throughout the entire material - the tiny gaps between particles themselves are distributed 'air gaps', and magnetic flux does not concentrate and overflow from any one location.

The second benefit is shape. Magnetic cores can be compressed into complex geometries with dispersed magnetic circuits, windings can be made into three-dimensional structures, or multiple magnetic functions can be integrated into one compact. This type of design has significant value in reducing volume and lowering assembly processes.

04Composition of losses and upper frequency limit

The loss of soft magnetic materials is often divided into three parts: hysteresis, eddy current, and residual (including resonance and relaxation). The characteristic of SMC is to "lock" eddy current losses inside the particles: the length of the eddy current path is limited by the particle size, and the losses generally increase with the square of the particle size and frequency, and increase with the decrease of material resistivity.

From this, we can understand the source of the upper frequency limit: as the frequency increases, eddy current losses increase by square; The coating layer also exhibits obvious capacitive characteristics at high frequencies, and the equivalent capacitance between particles intervenes in the dielectric behavior of the material at high frequencies, further increasing losses. This is also why SMC performs well in the frequency range of several hundred kHz to several MHz, and often gives way to ferrites beyond that.

Technological means Main suppressed losses cost
Refine particles eddy current loss The suppression density decreases, and the magnetic permeability and Bs decrease
Thickened insulation coating Eddy current and particle conduction An increase in non-magnetic phases leads to a decrease in magnetic permeability
Optimize annealing Hysteresis loss (reducing internal stress) Excessive temperature can damage the coating layer
Improve purity and consistency Heterogeneity and local hotspots Rising raw material costs

The choice in the third line is particularly delicate: annealing can reduce hysteresis loss, but the upper limit of annealing temperature for SMC is constrained by the temperature resistance of the coating layer. Once exceeded, the insulation is damaged and eddy current loss increases dramatically. The limitation of 'what seems like optimization cannot actually be done' is a typical difficulty in SMC technology.

05Typical applications and selection criteria

Application Reasons for choosing SMC Attention should be paid
Power inductor/energy storage Distributed air gap, less prone to local saturation under high current Low magnetic permeability, the number of turns needs to be increased
Common mode choke/EMI filtering High impedance characteristics and shape freedom The increase in high-frequency loss requires verification of the curve
Motor and Axial Flux Structure Three dimensional magnetic circuit, capable of suppressing complex tooth grooves Mechanical strength and compression density need to be balanced
Wireless charging and coupling structure Can be used as thin and irregular magnetic sheets The division of labor with flexible magnetic separators needs to be clearly defined

When selecting, you can ask three questions in order: what is the upper limit of the operating frequency, will the peak current saturate the magnetic core, and is the shape limited by standard components. The three answers will quickly point to a certain material - if the frequency is in the hundreds of kHz, the current is high, and an irregular structure is required, SMC is usually the preferred choice; If the frequency is high but the current is not large, ferrite is more cost-effective.

Soft magnetic composite materials may appear to exchange "low magnetic permeability" for "high frequency availability", but in reality, they also offer two design benefits: shape freedom and distributed air gaps. Understanding the role of the coating layer in this, one can understand why the parameter table of such materials always appears "ordinary", but repeatedly appears in power and EMI design.

For more technical information on soft magnetic composite materials, magnetic materials, and EMI related devices, please visitwww.avanzado.cn.

Contact

Contact us

Company:Xianjin Yuan (Shenzhen) Technology Co., Ltd.

Address: 8/F, Zhongxing Building, Shajing Xinsha Road, Bao'an District, Shenzhen, Guangdong, China

Tel: 0755-22277778   13826586185

Email: duanlian@xianjinyuan.cn

Hotline
0755-22277778
13826586185(Mr.Duan)
Wechat QRcode Wechat QRcode