The formula logic of low permeability absorbing materials: reduce μ, but cannot reduce the loss angle

Time:2026-11-27Number:7

Technical Note  /  Formulation Route

The most intuitive way to meet the demand for a low permeability absorbing material is to add less magnetic powder. The result of the experiment is usually that while the μ 'decreases from 100 to 40, the μ' also decreases from 30 to 12- the loss angle remains almost unchanged, but the absorption capacity has been halved.Because dilution proportionally weakens the real and imaginary parts, it does not make the material "more suitable for high frequencies", but only reduces it by one size.The key to the low magnetic permeability route is to suppress μ 'while preserving μ' as much as possible.

First, take a clear look at this trap before we can talk about what to do.

01Why dilution is an ineffective route

method μ′ μ″ Loss angle
Simply reduce filling decrease Proportional decline basically unchanged
Switching to higher frequency peak position powder decrease On the contrary, there is an increase in the target frequency band significantly improve
The combination of the two Reduce as required Maintain availability level in the target frequency band improve

The values in the table are mainly for illustration purposes, with a focus on the difference between the first and second rows: similarly, lowering μ 'to the target value only reduces the scale of one path, while changing the peak position of the other path. Therefore, the relative level of μ' in the target frequency band is different. What we really need to do in engineering is the second one.

Key points of the projectLow magnetic permeability is not about "reducing μ '", but about "increasing the tangent of the loss angle". The former is a side effect, while the latter is the goal.

02Four methods for reducing μ, each with its own side effects

means main function cost
Reduce the volume fraction of magnetic phase The most direct and simple process The year-on-year decline in μ "indicates a weakened absorption capacity
Introducing non-magnetic fillers Simultaneously regulate μ and ε to improve impedance More interfaces need to be redesigned and wrapped
Porosity/hollow microspheres Reduce density and significantly decrease ε Mechanical strength and thermal conductivity decrease, and compression is prone to rebound
Orientation and aspect ratio control Adjust anisotropy and change the in-plane μ and peak positions Narrow process window, high pressure for batch consistency

The third method is worth mentioning separately. One of the purposes of the low μ route is to improve impedance matching, which depends on the ratio of μ to ε, not just the decrease of μ alone. If μ decreases but ε does not decrease, the ratio may not necessarily be better; Introducing hollow microspheres or pores can simultaneously lower the pressure of both, resulting in a more significant improvement in matching. The density of this type of filler is usually significantly lower than that of solid magnetic powder, which also helps to reduce the overall weight of the piece.

But the cost is equally real: pores and hollow spheres make the material softer and more prone to collapse during compression or bonding, resulting in a decrease in mechanical strength and thermal conductivity. If the product also needs to undertake structural functions or be close to heat sources, this must be evaluated first.

03Three paths to preserve the loss angle

One is to choose the right powder.The natural resonance peak positions of powders with different particle sizes and alloy compositions are different. When the target frequency band is 5GHz, fine powders with resonance peaks already in the range of 4-8GHz should be selected, rather than relying on the tail support of low-frequency high μ powders. This determines the upper limit and cannot be compensated for by formula.

The second is multimodal mixing.Mixing two powders with different peak positions in proportion can maintain a usable μ "over a wider frequency range, at the cost of diluting both peaks. For low μ products, this dilution actually helps to flatten the losses.

The third is to maintain orientation.Flattening and magnetic field orientation can improve in-plane magnetic permeability and push peak positions higher, which is a bonus for "low μ but high frequency availability". However, the orientation process is sensitive to the filling rate, and after the filling is reduced, the particles are more likely to randomly flip during rolling, resulting in a reduced orientation effect - this is a difficult point that is often overlooked in low filling formulas.

The priority of the three paths is: first determine the powder, then determine the mixing, and finally adjust the filling. To do the opposite - first reduce the filling and then find the powder - usually involves repeated trial and error in several directions.

04Process changes caused by low filling

link change Need to confirm again
disperse The proportion of powder decreases, and the agglomeration effect is relatively amplified The peak of ε caused by single point aggregation is more pronounced
Rolling/Forming It is easier to press thin, but the consistency between rebound and thickness deteriorates Thickness tolerance control needs to be readjusted
orientation Under low filling, particles are prone to flipping and orientation decreases Magnetic field strength and process sequence need to be reset
Mechanical and Temperature Resistant Strength, thermal conductivity, and heat resistance may all decrease Structural functionality and applicability near heat sources

These changes mean that low μ is not a version that can be shipped by changing the ratio on the same production line. It often requires resetting the rolling pressure, orientation process, and thickness tolerance. If the supplier only lowers the filling ratio without adapting the process, the resulting product will be very "floating" - there are significant internal differences within the same batch, and different batches may not match.

05Four questions to ask in procurement

item Question Points I want to confirm
1 At the same time as the decrease in μ ', what is the value of μ' Does the loss angle really increase
2 Does ε 'decrease synchronously Has impedance matching truly improved
3 Have you undergone orientation treatment and what is the degree of orientation Does high-frequency loss depend on peak position rather than tail position
4 Does the mechanical strength and thermal conductivity meet the requirements for assembly Can the side effects caused by low filling be acceptable

The difficulty of formulating low permeability absorbing materials lies precisely in the fact that they cannot be completed by "subtraction". By lowering all parameters together, only a weaker material is obtained; Only by shifting the peak position upwards, raising the loss angle, and lowering the dielectric constant together can we obtain a low μ material that is truly suitable for high-frequency and tolerant bonding.

For more technical information on low permeability absorbing materials, flexible absorbing plate formulations, and high-frequency suppression schemes, please visitwww.avanzado.cn.

Contact

Contact us

Company:Xianjin Yuan (Shenzhen) Technology Co., Ltd.

Address: 8/F, Zhongxing Building, Shajing Xinsha Road, Bao'an District, Shenzhen, Guangdong, China

Tel: 0755-22277778   13826586185

Email: duanlian@xianjinyuan.cn

Hotline
0755-22277778
13826586185(Mr.Duan)
Wechat QRcode Wechat QRcode